Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | >= 0.44200 W/m-K @Temperature 350 °C |
>= 3.0625 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories C-2 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |