Polymer Property : Thermal Conductivity = 0.440 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 100 - 100 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.384 W/m-K Grade Count:15
Overview of materials for Phenolic, Novolac, Woodflour Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu..
Thermal Conductivity 0.440 - 0.440 W/m-K

@Temperature 100 - 100 °C
3.05 - 3.05 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.440 W/m-K Grade Count:1
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..