Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0605 W/m-K | 0.420 BTU-in/hr-ft²-°F | |
Saint-Gobain COHRlastic® F-12 Silicone Foam Description: Low-density, flame-retardant COHRlastic silicone foam yard goods provide outstanding performance for industries ranging from aviation and mass transit to automotive, electronics, constr.. |