Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0560 W/m-K | 0.389 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |