Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.294 W/m-K | 2.04 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |