Thermal Properties Metric English Comments
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
20 g/l; EN 12667
Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding
High quality processingHigh strengthLow wasteFast moulding cycles
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9335 MG 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 3%
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 4%
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Thickness 80.0 mm
0.243 BTU-in/hr-ft²-°F

@Thickness 3.15 in
DIN EN 13164
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 3%
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 4%
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Thickness 80.0 mm
0.243 BTU-in/hr-ft²-°F

@Thickness 3.15 in
DIN EN 13164
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 3%
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 4%
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Thickness 80.0 mm
0.243 BTU-in/hr-ft²-°F

@Thickness 3.15 in
DIN EN 13164
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Thickness 50.0 mm,
Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F

@Thickness 1.97 in,
Temperature 86.0 °F
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 3%
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 4%
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 3%
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 4%
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Thickness 80.0 mm
0.243 BTU-in/hr-ft²-°F

@Thickness 3.15 in
DIN EN 13164
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 3%
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 4%
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K

@Thickness 80.0 mm
0.243 BTU-in/hr-ft²-°F

@Thickness 3.15 in
DIN EN 13164
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..