Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.196 W/m-K | 1.36 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD10(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |