Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | >= 0.1861 W/m-K @Temperature 350 °C |
>= 1.289 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories A-4 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | >= 0.1861 W/m-K @Temperature 350 °C |
>= 1.289 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories LW-23 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |