Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.174 W/m-K | 1.21 BTU-in/hr-ft²-°F | |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Thermal Conductivity | >= 0.174 W/m-K @Temperature 350 °C |
>= 1.21 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories A-3 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | >= 0.174 W/m-K @Temperature 350 °C |
>= 1.21 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories LW-20 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |