Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.156 W/m-K | 1.08 BTU-in/hr-ft²-°F | |
Pyrotek Pyroboard™ S1090 Roller Pyroboard™ S1090 is used in cooling and preheat areas of the furnace where the temperature does not exceed 1600° F.Information provided by Pyrotek. |
|||
Thermal Conductivity | 0.156 W/m-K | 1.08 BTU-in/hr-ft²-°F | |
Trelleborg AEM Syntac® Eccolite® Ultra Eccolite® Ultra is a new generation syntactic foam plug assist material, a new thermoplastic compound developed in response to the needs of the thermoforming industry. Eccolite® is tough and robus.. |
|||
Thermal Conductivity | 0.156 W/m-K | 1.08 BTU-in/hr-ft²-°F | |
Trelleborg AEM Syntac® 450 Syntactic Foam Syntac® 450 syntactic foam is the high temperature (450°F/232°C) member of the Syntac® product family.A rigid, high strength composite of epoxy resin and hollow glass microspheres, Syntac® 450 .. |