Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.136 W/m-K @Thickness 6.35 mm, Temperature 43.3 °C |
0.944 BTU-in/hr-ft²-°F @Thickness 0.250 in, Temperature 110 °F |
|
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |