Thermal Conductivity 0.122 W/m-K
0.847 BTU-in/hr-ft²-°F
Melt
Covestro Desmopan® DP 9370A Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi..