Polymer Property : Thermal Conductivity = 0.111 BTU-in/hr-ft²-°F
Polymer Property :
Thermal Conductivity =
0.111 BTU-in/hr-ft²-°F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.0160
W/m-K
0.111
BTU-in/hr-ft²-°F
In Air
MarkeTech Silica Aerogel
Silica aerogels are generally known for being an extremely lightweight transparent solid down to