Polymer Property : Thermal Conductivity = 0.0830 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0830 W/m-K

@Temperature 150 °C
0.576 BTU-in/hr-ft²-°F

@Temperature 302 °F
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Thermal Conductivity 0.0830 W/m-K

@Temperature 150 °C
0.576 BTU-in/hr-ft²-°F

@Temperature 302 °F
measured on 10 mil sample
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Thermal Conductivity 0.0830 W/m-K

@Temperature 150 °C
0.576 BTU-in/hr-ft²-°F

@Temperature 302 °F
measured on 10 mil sample
DuPont™ Nomex® E56 Paper, 15 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Thermal Conductivity 0.0830 W/m-K

@Temperature 150 °C
0.576 BTU-in/hr-ft²-°F

@Temperature 302 °F
measured on 10 mil sample
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Thermal Conductivity 0.0830 W/m-K

@Temperature 150 °C
0.576 BTU-in/hr-ft²-°F

@Temperature 302 °F
measured on 10 mil sample
DuPont™ Nomex® E56 Paper, 5 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Thermal Conductivity 0.0830 W/m-K

@Temperature 150 °C
0.576 BTU-in/hr-ft²-°F

@Temperature 302 °F
measured on 10 mil sample
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..