Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0457 - 0.0530 W/m-K
0.317 - 0.368 BTU-in/hr-ft²-°F
Beijing Evergrow Resources GFF-5 Glass Fiber Felt
Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a..