Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0280 W/m-K @Temperature -40.0 °C |
0.194 BTU-in/hr-ft²-°F @Temperature -40.0 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0280 - 0.0320 W/m-K | 0.194 - 0.222 BTU-in/hr-ft²-°F | |
Beijing Evergrow Resources GFF-10 Glass Fiber Felt Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a.. |
|||
Thermal Conductivity | 0.0280 W/m-K @Temperature -40.0 °C |
0.194 BTU-in/hr-ft²-°F @Temperature -40.0 °F |
|
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0280 W/m-K @Thickness 50.0 mm, Temperature -40.0 °C |
0.194 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature -40.0 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0280 W/m-K @Temperature -40.0 °C |
0.194 BTU-in/hr-ft²-°F @Temperature -40.0 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0280 W/m-K @Temperature -40.0 °C |
0.194 BTU-in/hr-ft²-°F @Temperature -40.0 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0280 W/m-K @Temperature -40.0 °C |
0.194 BTU-in/hr-ft²-°F @Temperature -40.0 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |