Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 176 °C @Thickness <=0.102 mm |
349 °F @Thickness <=0.00400 in |
TMA; ASTM D3850 |
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a .. |