Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 172 °C @Thickness <=0.0508 mm |
342 °F @Thickness <=0.00200 in |
TMA; ASTM D3850 |
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a .. |