Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 86.4 - 179 µm/m-°C | 48.0 - 99.6 µin/in-°F | Average value: 139 µm/m-°C Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |