Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.6 - 98.0 µm/m-°C | 7.00 - 54.4 µin/in-°F | Average value: 41.5 µm/m-°C Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |