Thermal Properties Metric English Comments
CTE, linear 172 µm/m-°C

@Temperature 20.0 °C
95.6 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Spartech PP5140 Talc Filled Homopolymer
Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech