Polymer Property : CTE, linear = 94.0 µin/in-°F
Polymer Property :
CTE, linear =
94.0 µin/in-°F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
CTE, linear
169
µm/m-°C
94.0
µin/in-°F
Aremco Aremco-Bond™ 2330 High Performance Epoxide
Single-Part, Heat Curable, Silicone Elastomer Adhesive