Thermal Properties Metric English Comments
CTE, linear 87.1 µm/m-°C
48.4 µin/in-°F
Below Tg
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System
TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and ..