Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.5 µm/m-°C @Temperature 204 °C |
8.60 µin/in-°F @Temperature 400 °F |
with ply; 8HS form; ASTM D696 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
CTE, linear | 15.5 µm/m-°C | 8.60 µin/in-°F | |
Weartech International WT-40 Nickel Hardfacing & Wear Resistant Alloy Applications: glass industry plungers and mold componentsInformation provided by Weartech International |