Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.39 µm/m-°C @Temperature 20.0 - 650 °C |
4.66 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Du-Co Ceramics DC-16-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |