Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 143 µm/m-°C @Temperature 20.0 °C |
79.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
CTE, linear | 143 µm/m-°C | 79.4 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® H31D-LV Epoxy Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i.. |