Thermal Properties Metric English Comments
CTE, linear 7.00 - 138 µm/m-°C
3.89 - 76.7 µin/in-°F
Average value: 36.4 µm/m-°C Grade Count:5
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..