Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.326 - 730 µm/m-°C | 0.181 - 406 µin/in-°F | Average value: 238 µm/m-°C Grade Count:35 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |