Polymer Property : CTE, linear = 730 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 730 µm/m-°C
406 µin/in-°F
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT
Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning