Polymer Property : CTE, linear = 73.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 131 µm/m-°C

@Temperature 20.0 °C
73.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Tefzel® 2181 ETFE
Products made from Tefzel® HT-2181 resin are suitable for a variety of processes and demanding end uses. They are mechanically tough and offer an excellent balance of properties. These products p..