Polymer Property : CTE, linear = 70.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 70.6 µm/m-°C
39.2 µin/in-°F
BCC Products MB 8250 Aluminum Board
MB 8250 is an aluminum filled product that is dimensionally stable and exhibits great machinable properties. Features: excellent machineability, low dust emission, no shrinkage, low moisture absorp..