Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.80 - 7.20 µm/m-°C @Temperature 20.0 - 100 °C |
3.78 - 4.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech Cu/Mo/Cu 1:4:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |