Thermal Properties Metric English Comments
CTE, linear 12.8 µm/m-°C

@Temperature 20.0 °C
7.11 µin/in-°F

@Temperature 68.0 °F
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 13%.
CTE, linear 12.8 µm/m-°C

@Temperature 20.0 - 100 °C
7.11 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals INCONEL® Alloy 625
Niobium content includes tantalum. A nickel-chromium-molybdenum alloy with an addition of niobium that acts with the molybdenum to stiffen the alloy's matrix and thereby provide high strength witho..
Copyright © lookpolymers.com All Rights Reserved