Thermal Properties Metric English Comments
CTE, linear 101 - 121 µm/m-°C

@Temperature 20.0 °C
56.0 - 67.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..