Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 63.2 µm/m-°C | 35.1 µin/in-°F | |
Atom Adhesives AA-BOND F123 Epoxy Adhesive AA-BOND F123 is a low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating single or multi.. |
|||
CTE, linear | 63.2 µm/m-°C | 35.1 µin/in-°F | |
Atom Adhesives AA-BOND F123BK Epoxy Adhesive AA-BOND F123BK is a low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating single or mul.. |