Polymer Property : CTE, linear = 62.7 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 62.7 µm/m-°C
34.8 µin/in-°F
Below Tg
Tra-Con Tra-Bond F253 Color Keyed High Temperature Epoxy Adhesive
TRA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status. The unmixed components are light yellow; the mixt..