Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 109 µm/m-°C @Temperature 35.0 - 172 °C |
60.6 µin/in-°F @Temperature 95.0 - 342 °F |
ASTM E831 |
Proto3000 Duraform® AF Selective Laser Sintering (SLS®) Prototyping Polymer Description: Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use.Features:Metallic appearance with nice surface finishGood powder recycle character.. |
|||
CTE, linear | 109 µm/m-°C | 60.6 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 320-3 Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
CTE, linear | 109 µm/m-°C @Temperature 35.0 - 172 °C |
60.6 µin/in-°F @Temperature 95.0 - 342 °F |
ASTM E831 |
3D Systems DuraForm® AF Nylon for SLS® Systems Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use. For use with all selective laser sintering SLS® systems.ApplicationsHousings and enclosuresCo.. |
|||
CTE, linear | 109 - 109 µm/m-°C @Temperature 55.0 - 160 °C |
60.6 - 60.6 µin/in-°F @Temperature 131 - 320 °F |
Average value: 109 µm/m-°C Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |