Polymer Property : CTE, linear = 6.911 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 12.44 µm/m-°C

@Temperature 20.0 - 217 °C
6.911 µin/in-°F

@Temperature 68.0 - 423 °F
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022
AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide..