Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.9 µm/m-°C | 6.61 µin/in-°F | at Set Pt. |
Ferro EG 2760 Thick Film Glass Glass Type: Pb-B-Zn Typical Powder Form: MVG, VEG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduc.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 300 °C |
6.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott S8809 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 93.0 °C |
6.61 µin/in-°F @Temperature 199 °F |
|
Special Metals UDIMET® alloy 188 Cobalt-base Alloy UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small .. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 93.0 °C |
6.61 µin/in-°F @Temperature 199 °F |
|
Special Metals UDIMET® alloy R41 Ni-Cr Alloy UDIMET® alloy R41 (UNS N07041) is a precipitation-hardenable nickel-chromium alloy containing significant amounts of cobalt and molybdenum, along with lesser amounts of aluminum and titanium. Al.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 100 °C |
6.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling syst.. |