CTE, linear 1000 µm/m-°C
556 µin/in-°F
3M Fluorinert™ FC-70 Electronic Liquid
Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a..