Thermal Properties Metric English Comments
CTE, linear 10.6 µm/m-°C

@Temperature 21.1 - 538 °C
5.89 µin/in-°F

@Temperature 70.0 - 1000 °F
PSM Industries Ferro-TiC® SK Impact Resistant Tool Steel
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce..
CTE, linear 10.6 µm/m-°C

@Temperature 20.0 - 200 °C
5.89 µin/in-°F

@Temperature 68.0 - 392 °F
Crucible Steel CPM® 3V® Tool Steel
CPM 3V is a new tool steel made by the Crucible Particle Metallurgy process, designed to provide maximum resistance to breakage and chipping in a highly wear-resistant steel. CPM 3V offers impact to..
CTE, linear 10.6 µm/m-°C

@Temperature 93.3 °C
5.89 µin/in-°F

@Temperature 200 °F
ATI Allegheny Ludlum AL 13-8™ H 1100 Precipitation Hardening Alloy
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..
CTE, linear 10.6 µm/m-°C

@Temperature 93.3 °C
5.89 µin/in-°F

@Temperature 200 °F
ATI Allegheny Ludlum AL 13-8™ H 950 Precipitation Hardening Alloy
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..
CTE, linear 10.6 µm/m-°C

@Temperature 20.0 - 100 °C
5.89 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum AL 13-8™ H 1000 Precipitation Hardening Alloy
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..
CTE, linear 10.6 µm/m-°C

@Temperature 93.3 °C
5.89 µin/in-°F

@Temperature 200 °F
ATI Allegheny Ludlum AL 13-8™ H 1025 Precipitation Hardening Alloy
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..
CTE, linear 10.6 µm/m-°C

@Temperature 20.0 - 100 °C
5.89 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1050°F
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..
CTE, linear 10.6 µm/m-°C

@Temperature 20.0 - 100 °C
5.89 µin/in-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..