Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.70 - 6.10 µm/m-°C @Temperature 20.0 - 100 °C |
3.17 - 3.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
CTE, linear | 5.70 µm/m-°C @Temperature 20.0 - 320 °C |
3.17 µin/in-°F @Temperature 68.0 - 608 °F |
|
Corning Pyroceram® Glass Ceramic High strength, high elastic modulus, and uniform dielectric properties. Pyroceram® can be manufactured in ogival ( pointed arch) shapes, hemispheres, pressware sheets, and various machined shapes. .. |
|||
CTE, linear | 5.70 µm/m-°C @Temperature 1000 °C |
3.17 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CH-1 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.70 µm/m-°C @Temperature 1000 °C |
3.17 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories N4-1 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.70 µm/m-°C @Temperature 1000 °C |
3.17 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories N4-2 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |