Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.59 µm/m-°C @Temperature 20.0 °C |
3.11 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Yttrium Aluminate (YAlO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |