Thermal Properties Metric English Comments
CTE, linear 47.5 µm/m-°C
26.4 µin/in-°F
MarkeTech Sodium Iodide:Thallium (Nal:Tl) Scintillator Crystal
Sodium iodide activated by thallium has long been the scintillation standard. Nal:Tl has good performance, economical price, high luminescence efficiency, very good spectroscopic performance and no ..