Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 84.2 µm/m-°C | 46.8 µin/in-°F | |
BCC Products MB 2001 Urethane Foam Modeling Board MB2001 is a general purpose light weight urethane board engineered specifically to meet the tooling requirements of a wide range of applications for the automotive/aerospace, prototype, foundry, and.. |