Polymer Property : CTE, linear = 44 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 80 µm/m-°C

@Temperature 20.0 °C
44 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Kolon SPELLOY® KB133HF PC + PBT Alloy Resin  (discontinued **)
SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional..