Thermal Properties Metric English Comments
CTE, linear 15.0 - 42.3 µm/m-°C
8.33 - 23.5 µin/in-°F
Average value: 24.0 µm/m-°C Grade Count:31
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..