Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 72.5 µm/m-°C | 40.3 µin/in-°F | Below Tg |
Tra-Con Tra-Bond FS437 Low Viscosity High Impact Epoxy Adhesive TRA-BOND FS437 is a two-part, low viscosity material formulated for optical applications which require excellent wicking, visible color and high strength. This material has been used successfully fo.. |