Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.61 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 µin/in-°F @Temperature 68.0 - 752 °F |
|
Hogen HM1100 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers hig.. |
|||
CTE, linear | 4.61 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 µin/in-°F @Temperature 68.0 - 752 °F |
|
Mi-Tech Metals HD17D Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The t.. |