Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.92 µm/m-°C @Temperature 20.0 °C |
4.40 µin/in-°F @Temperature 68.0 °F |
|
Pyrotek Pyrocast ZI Refractory Shapes Aggregate Base: BauxiteApplicationsCrucible bottoms Information provided by Pyrotek. |